kw.\*:("nanoindentation")
Results 1 to 25 of 2351
Selection :
Development of reference materials for the investigation of local mechanical properties at the nanoscaleCAMPBELL, Anna Charvátová; KLAPETEK, Petr; VALTR, Miroslav et al.Surface and interface analysis. 2012, Vol 44, Num 8, pp 1151-1154, issn 0142-2421, 4 p.Conference Paper
An experimental/computational approach to identify moduli and residual stress in MEMS radio-frequency switchesESPINOSA, H. D; ZHU, Y; FISCHER, M et al.Experimental mechanics. 2003, Vol 43, Num 3, pp 309-316, issn 0014-4851, 8 p.Article
Measurement of creep compliance of solid polymers by nanoindentationLU, H; WANG, B; MA, J et al.Mechanics of time-dependant materials. 2003, Vol 7, Num 3-4, pp 189-207, issn 1385-2000, 19 p.Article
Effects of diffusion on interfacial fracture of gold-chromium hybrid microcircuit filmsMOODY, N. R; ADAMS, D. P; MEDLIN, D et al.International journal of fracture. 2003, Vol 119-20, Num 4/1-2, pp 407-419, issn 0376-9429, 13 p.Article
Atomic force microscopy and nanoindentation characterization of human lamellar bone prepared by microtome sectioning and mechanical polishing techniqueXU, J; RHO, J. Y; MISHRA, S. R et al.Journal of biomedical materials research. 2003, Vol 67A, Num 3, pp 719-726, issn 0021-9304, 8 p.Article
Cluster Issue on IndentationMUNAWAR CHAUDHRI, M; YONG YEE LIM.Journal of physics. D, Applied physics (Print). 2008, Vol 41, Num 7, pp 070301.1-074029.7, issn 0022-3727Conference Proceedings
Evolution of the mechanical properties of a femtosecond laser modified layer onto a silicon waferVALETTE, S; BENAYOUN, S.Applied surface science. 2013, Vol 279, pp 62-66, issn 0169-4332, 5 p.Article
Study of nanoindentation behavior of amorphous alloy using molecular dynamicsCHEN QIU; PENGZHE ZHU; FENGZHOU FANG et al.Applied surface science. 2014, Vol 305, pp 101-110, issn 0169-4332, 10 p.Article
Nanohardness, corrosion and protein adsorption properties of CuAlO2 films deposited on 316L stainless steel for biomedical applicationsCHANG, Shih-Hang; CHEN, Jian-Zhang; HSIAO, Sou-Hui et al.Applied surface science. 2014, Vol 289, pp 455-461, issn 0169-4332, 7 p.Article
Effects of viscoelasticity and time-dependent plasticity on nanoindentation measurements of human cortical boneZAIFENG FAN; RHO, Jae-Young.Journal of biomedical materials research. 2003, Vol 67A, Num 1, pp 208-214, issn 0021-9304, 7 p.Article
Evaluation of the substrate effect on indentation behavior of film/substrate systemWANG, J. S; ZHENG, Xj; ZHENG, H et al.Applied surface science. 2010, Vol 256, Num 20, pp 5998-6002, issn 0169-4332, 5 p.Article
On the fundamental relation used in nanoindentation with piecewisely defined indentersGUANGHUI FU; TIESHENG CA.Materials science & engineering. A, Structural materials : properties, microstructure and processing. 2009, Vol 513-514, pp 276-278, issn 0921-5093, 3 p.Article
Mechanical characterisation of wood-adhesive interphase cell walls by nanoindentationKONNERTH, Johannes; GINDL, Wolfgang.Holzforschung. 2006, Vol 60, Num 4, pp 429-433, issn 0018-3830, 5 p.Article
Effect of cold work on surface reactivity and nano-hardness of alloy 800 in corroding environmentsZHU, R. K; LU, B. T; LUO, J. L et al.Applied surface science. 2013, Vol 270, pp 755-762, issn 0169-4332, 8 p.Article
Mechanical and electrical properties of GeSb2Te4 film with external voltage appliedCHENG, Guang-Gui; ZHANG, Zhong-Qiang; DING, Jian-Ning et al.Applied surface science. 2013, Vol 285, pp 532-537, issn 0169-4332, 6 p., bArticle
Structure and surface nanomechanics of poly(r-lactide) from thermally induced phase separation processJUNDONG SHAO; CONG CHEN; YINGJUN WANG et al.Applied surface science. 2012, Vol 258, Num 17, pp 6665-6671, issn 0169-4332, 7 p.Article
Molecular dynamic simulations of nanoindentation in aluminum thin film on silicon substratePING PENG; GUANGLAN LIAO; TIELIN SHI et al.Applied surface science. 2010, Vol 256, Num 21, pp 6284-6290, issn 0169-4332, 7 p.Article
Pilot investigation of the mechanical properties of wood flooring paint films by in situ imaging nanoindentationZEHUI JIANG; YAN YU; DAOCHUN QIN et al.Holzforschung. 2006, Vol 60, Num 6, pp 698-701, issn 0018-3830, 4 p.Article
Effects of small indenter size and its position on incipient yield loading during nanoindentationWENSHAN YU; SHENGPING SHEN.Materials science & engineering. A, Structural materials : properties, microstructure and processing. 2009, Vol 526, Num 1-2, pp 211-218, issn 0921-5093, 8 p.Article
Nanotribological performance of fullerene-like carbon nitride filmsFLORES-RUIZ, Francisco Javier; ENRIQUEZ-FLORES, Christian Ivan; CHINAS-CASTILLO, Fernando et al.Applied surface science. 2014, Vol 314, pp 193-198, issn 0169-4332, 6 p.Article
The joint effect of laser and shear stress treatments for the surface strengthening of Zr alloysWEI ZHAO; JIAN LI; XIAO JIANG et al.Applied surface science. 2013, Vol 286, pp 379-383, issn 0169-4332, 5 p.Article
Nanoindentation and nanoscratch behaviors of Ag/Ni multilayersWEN, S. P; ZONG, R. L; ZENG, F et al.Applied surface science. 2009, Vol 255, Num 8, pp 4558-4562, issn 0169-4332, 5 p.Article
Instrumented indentation testing in materials research and developmentJENNETT, Nigel M; PHARR, George M; MCHARGUE, Carl J et al.Philosophical magazine (2003. Print). 2006, Vol 86, Num 33-35, issn 1478-6435, 618 p.Conference Proceedings
AFM nanoscale indentation in air of polymeric and hybrid materials with highly different stiffnessSURIANO, Raffaella; CREDI, Caterina; LEVI, Marinella et al.Applied surface science. 2014, Vol 311, pp 558-566, issn 0169-4332, 9 p.Article
Elasto-plastic characteristics and mechanical properties of as-sprayed 8 mol% yttria-stabilized zirconia coating under nano-scales measured by nanoindentationLUO, J. M; DAI, C. Y; SHEN, Y. G et al.Applied surface science. 2014, Vol 309, pp 271-277, issn 0169-4332, 7 p.Article